    Hi, All in Ganoksin! I have been a subscriber, and a lurker only, for
    several months now. I've gotten so much good infor from reading the
    postings & answers when I have the time. Okay, on to my first posting
    & wonderment: 

    I was away from the Bench for about 8 years, and went back to work
    this past January. In my 'time off', white gold changed, as you all
    must well know. So now I find myself having an issue with my sizing
    joints in the white gold rings- verrrrry frustrating! I use an
    acetylene/oxy torch and Hoover & Strong solder. I *used* to use 20K
    white hard for sizings, but am having a bit more luck now with 14K
    white hard. But, a certain percentage of them still show up after
    polishing. I'm using the same technique I always did, but don't
    remember having this much trouble with them 'popping up'. My seams
    are flush & clean, my heating of the piece even, good flux
    application.....I m perplexed. 

    Anyone have any tips? I'm open to any & all suggestions. Thanks in
    advance- 

Tracy Brown

 
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project