    Hello Raakhi. Since you seem a little confused..... There are a few
    rings that just cannot be sized - tungsten carbide, for instance.
    Just about any other ring in the normal world can be, one way or
    another. The question is, what is that way? There's no way to know
    that exactly without seeing the actual ring, and what's to be done.
    Size up? Down? How much? and when you say filagree, what does that
    mean? Many people use the word for simple fine piercing. Sometimes
    you'll just have to live with a place where it's sized that's neat,
    but different from the pattern. Engraving can always just be
    re-engraved, if it's on the outside - not some message on the inside,
    though. Sizing balls are a generic term for things that are soldered
    on the inside of the ring to tighten it up - sometimes it's 2 little
    balls at 5 and 7 O'clock, sometimes it's a small bar of gold, and the
    ultimate is a 3/4 ring of spring gold soldered inside. They are not
    actually intended for sizing, though they work, somewhat. They are
    more for arthritic knuckles or just big knuckles, so the ring doesn't
    spin after it's on. I'd suggest finding a quality jeweler, and have 
it
    sized properly, if necessary. You'll be happier in the long run...
    And, you never know, it just might fit out of the box... 

http://www.donivanandmaggiora.com
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project