    Hello, this is really hard to say without seeing the stone. Even then
    it is sort of a guess. Is the prong putting crooked or excessive
    pressure on the stone? Is the inner edge of the prongs rubbing up
    against the girdle in an stressing way? You really want the prong to
    hold the contour of the stone without putting any real pressure on
    any edges or points. Prongs should really just frame a stone. This
    is hard to do, really well. with diamonds you can sort of get away
    with excessive pressure but on colored stones you are more apt to put
    uneven pressure. If it were me depending on the answers to the above
    questions, I would perhaps back the prong off a bit from the girdle
    edge. It is always a scary venture once you have caused something to
    go amiss, it is hard to know when to stop fiddling. Is this an
    emerald cut? Aqua's often are, and they are harder to set, at least
    for me. 

good luck,
Dennis
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project