========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== I only just mentioned this before. For small amounts of metal, like under 8 dwts. or so, I make ingots on a charcoal block with self-locking tweezers. I have 3 ingot molds, and crucibles and melting dishes, too. If you get those nickel plated tweezers with the wider tips, not the skinny, red handled variety, then melt your button till it's just fluid, and straddle it with the tweezers and close them some, the metal will run along the tips, making a long ingot. It's difficult to describe, but very simple to do. Dip the tweezers in water first. Also, any ingot will benefit from fire-polishing, which is when you heat enough to melt the surface, but not to melt the core of the metal. Makes it nice and smooth. http://www.donivanandmaggiora.com ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project