    I have a hard time fabricating a way to make silver ingots that come
    out close to the right size to work with my roller. If I use the ones
    I have purchased for this, they are to thick and I end up either
    filing a considerable amount off, or annealing and using a hammer and
    anvil to get them down to size. I don't like doing either, and both
    are probably the wrong thing to do. 

    I have tried using casting sand to make an open, one sided form of
    my correct size, but am having troubles getting the amount of silver
    correct. The end product is either budged to high on top, or sunken.
    Will this way work, and is there a good way to figure how much
    material I need to fill the fabricated mold? 

    These are just ways I have tried on my own, and I have no idea if
    they are even close to anything correct or even workable. So I am
    open to any and all suggestions on making this. I don't really have
    the money to buy anything else right now, and I am already looking
    into a place to send my silver scrap to possibly trade for stock,
    especially being made aware of the drawbacks, thanks again Orchid, to
    working used silver. 

Thanks
Dan
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project