    Georgie, you get my vote for the most intrepid Orchidian out there.
    But your difficulties could be many things. My drawplates do go
    in.5mm increments - there's a .25 here and there. You need some big
    stout pliers, if not official draw tongs. And you must use
    lubrication - we use Vaseline. In tubing, it's easy to draw it, until
    the edges meet, and then it gets really, really hard to draw - it's
    like a 2mm wire, which is a lot to draw. I try to make it "perfect" -
    so the edges meet at the size I want, then I give it one last pull,
    for roundness. Trying to reduce the size IS difficult. Also, your
    troubles could be related to the taper of the holes on the backside.
    They need to be very smooth and even. I do congratulate you for
    making a drawplate out of wood - realize that the forces involved
    are extreme - it may have a fairly short life... 

        I must apologize - I replied to this before <above>- most of it
        was (hopefully) useful. But I just pulled some wire, and my
        recollection was wrong. It's a carbide drawplate from 2.8mm to
        tiny, and the holes aren't.5 mm, they are.1mm steps - quite a
        difference, and a couple are.05mm. 

http://www.donivanandmaggiora.com
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project