Hi Chaya,

    I actually did this recently by mistake, so this is my experience
    only. I'd never read anything about it, it just happened! I had been
    working on experimenting with fusing a ring using some extra 14k
    peach gold from some sprues. Whenever I have been trying to fuse 14k
    gold, I use flux. So this was my process - flux, fuse, pickle,
    forge, anneal, forge, anneal, forge, little extra flux to fuse
    again, pickle, forge..... some more of the above - then then last
    round of flux - fuse and pickle, I took it out and it had turned
    yellow - no longer had the peachy glow. it was really just all of a
    sudden and I was pretty shocked by it at first. 

    That was my process, and if I repeated those, I don't know for sure
    if it would work again, but I tend to think it would. As far as
    bringing the copper up, are you sure your pickle is fresh and
    untainted? I have found that if my pickle is even slightly off the
    14k copper plates before my sterling does. 

Hope that helps!
Beth
www.bethcyr.com
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project