    Many of the suppliers for the lampwork glass bead people carry the
    dichroic glass in sheets and "sticks". You must get all the same type
    of glass with the same co-efficiency of expansion in order to be able
    to fuse colors together or fuse with other glass of the same type.
    When ordering, ask if all the glass that you are purchasing is
    compatible. This will preclude incompatibility so that you will not
    have problems after you fire such as the glass of it coming apart or
    exploding. Also, make sure that you ask at what temperature should
    this glass be fired. If the wrong temperature is used, the dichroic
    can burn off. You might also go to the library and make inquiry about
    a book using dichroic glass. There are many books published on this
    subject. Among some of those are FrantzArtGlass.com and also
    glasscraft.com. Both are reliable companies (no affiliation etc.). 

Beth Katz
Unique Solutions, Inc.
Paste Solder and Powder Solder for Jewelers and Metalsmiths
www.myuniquesolutions.com
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project