From: Gerald
Date: Wed Oct 04 07:44:30 2006
 
     
========[ Invite a Friend - http://www.ganoksin.com/invite.htm  ]========

    To further this, a Toronto wholesaler was casting rings in 12KT.
    Until someone did a metallurgy test and saw the major problem. Many 
of
    the stores he sold to were stuck with his jewellery (sic). All of a
    sudden, he wondered why no one was buying from him. He closed down
    his business. Selling without a trademark and a karat stamp is a
    Canadian and a RCMP offense. No messing around with the Canadian
    Gov't Laws and Ottawa guys. Also...I once worked with a fellow who
    cast all of his jewellery in 14 1/4 karat just in case of an error in
    the alloy mix. He never lost money for the extra 1/4 Kt., but kept
    his customers happy and secure. These days you can't be too
    careful...! 

Gerry!
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project