========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Hello...........By way of introduction.....a tip. When casting, shrinkage is, for the most part, expansion of the investment during burnout. To reduce the expansion immerse the mold in 105F water immediately after pouring the investment. Leave it in the water until it sets. I use a 5 gallon aquarium with a heater so the temp stays constant. I learned this trick 35 years ago when I set up a dental lab and was casting crowns. They have to fit perfectly the first time. I've not found an investment that this doesn't work with but try it on a non critical piece first. Chris Find me on Google Earth 45 43'03.24"N 123 53'45.81"W ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project