From: Elaine Luther Date: Wed Sep 06 03:16:29 2006 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== > What else can I do? Any further advice would be appreciated. I > want to make another orca and try again, but not until I know I can > solder it right. Ah, welcome to being a jeweler. What can you do? Practice, practice, practice, practice. Can you find someone experienced to watch you solder? Students can tell me, but I did everything right, but then I sit with them as they solder and watch them and I can help them fix what they're doing wrong. Usually it's uneven heating. Elaine. Elaine Luther Metalsmith, Certified PMC Instructor http://www.CreativeTextureTools.com (TM) Hard to Find Tools for Metal Clay ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project