From: andy cooperman Date: Sun Sep 03 00:58:35 2006 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== You can use sand, glass beads from a bead blaster, etc. I seal the ends with wax. I've also filled the tube with water (sealing the ends with wax) and froze it. This works well, but leave space for the water to expand as it freezes. There is also a variety of low fusing metal alloys-- bizmuth and tin, I think-- that can be melted in boiling water, poured into the tube, left to harden and then melted out in boiling water after the tube is bent. Cerrobend is one of these. Just google it. Andy ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2007, The Ganoksin
Project