Re: [Orchid] Beware - Orange Peel on Palladium  
  [Thread Prev] [Message Prev]      [Date Index]   [Thread Index]      [Message Next] [Thread Next]
From: Paul Finelt
Date: Thu Aug 31 00:40:17 2006
 
     
========[ Invite a Friend - http://www.ganoksin.com/invite.htm  ]========

Thomas.

    Orange peel is generally the result of large grain size. If the Pd
    parts were over annealed or not sufficiently worked to reduce the
    grain size, the 'plating' might just be 'bringing out' the coarse
    underlying structure. Sanding and repolishing won't eliminate the
    structure at this point. If you put a very heavy/expensive rhodium
    plating you might cover the large grain structure. 

    Palladium will require some adjustments to your shop practice. Does
    that make sense? All (precious) metals are not created equal. 

    EVERYONE should check out
    http://www.ganoksin.com/borisat/nenam/950Palladium-earrings.htm and
    http://www.palladiumcoins.com if you are doing any work in palladium.

Paul Finelt
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project