| Re: [Orchid] First Argentium Sterling Adventure | ||
|
[Thread Prev]
[Message Prev]
[Date Index]
[Thread Index]
[Message Next]
[Thread Next]
From: Jaye Lewis Date: Thu Aug 10 22:39:46 2006 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== > This is great news, and with mud in my face I apologize for the > erroneous info I passed along. Well gosh Thackeray, you've gone and thrown me through the loops! Kidding, but I noticed that the activation temp and time has gone from 300 degrees for 30 minutes down to 250 for 10? Also, since you've tapped on affecting the activation through working the material, that would mean finish all the way up to pre-setting or just set/polish/bake and hope your stones don't mind? 250 degrees does sound better than 300 if this is the case. Even if it's not hot enough to bake a pizza. ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project