Dear all,

    How about this: my necklaces are fine at the crimp. They break
    someplace else on the strand. I have been trying to figure out why
    this has happened. All of a sudden, about a month ago, four of my
    favorite necklaces all broke within days of each other. They were all
    strung on tigertail, Beadalon bead stringing wire, nylon coated
    stainless steel, .018", 20 lbs. 

    These necklaces were not heavy. All three were strung with semi
    precious beads, and two had small silver medallions hanging from the
    center. Two broke in the front, and the one of only beads, broke on
    the side. They were all strung about two years ago, around the same
    time. I take this to mean that this wire has a life of about two
    years. I am also thinking that perhaps perfume oil, body lotion, may
    degrade the strength of the nylon coating? I wonder about that
    though, because I have a bracelet I made at the same time, that has
    not broken, and I wear it everyday, never take it off...bite my
    tongue!!! 

    Any thoughts? Ant similar experiences? 

Best,
Bayla
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project