    I buy my clear quartz in rods and cut it to the proper thickness for
    making triplets. I cut it about 1.5 mm, then flatten the cut side on
    a flat lap. 

    I buy it from http://www.creativegems.com

    Creative Gems
    P.O. Box 518
    Seagoville, Tx 75159

    Toll Free 1-888-287-3445
    Fax 972-427-9907

    A rod is $6.00, 6+ inches long, and about.5 inch to.75 inch in
    width. I have had great customer service, including over night
    shipping when I was in a triplet making class in Grady and Phyllis are
    wonderful people and I'm sure you will be happy with their product
    and service. They also have (or used to have) precut and pre-shaped
    caps in different sizes for triplets if you don't want to have to cut
    them, but I prefer the rods, much more versatile. 

Love and God Bless
randy
http://www.rocksmyth.com
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project