From: coralnut Date: Fri Aug 04 00:43:33 2006 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Vera....goodness there is no reason to be intimidated by casting. There are certain protocols to be followed of course, but by and large everything is pretty much above board. Both vacuum and centrifuge casting are quite safe if the protocols are followed. At the school, we once had a cracked investment and when we cast all the metal shot straight through the flask....nearly 5 oz of it. Guess what? The entire load was captured in the flask holder....not one drop went outside the holder or the tub. Casting with a torch is no different than soldering in terms of danger. Don't let it intimidate you. I have cast at the school and in my home for years with no problems. Take a class, study up a bit and just do it! You'll love it. Cheers from Don at The Charles Belle Studio in SOFL where simple elegance IS fine jewelry! dcdietz AT comcast.net ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project