========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== The product that Beth Katz mentioned is probably as good as it gets;however, if you don't have any, you might try what I use. To stop solder from flowing out from under a bezel cup, when necessary, I usually just use a "Sharpie" marker. If I need to cover a larger area, I just take a small brush and dip the tip into alcohol and then swip it across my red rouge several times to coat the brush tip and paint away.Just remember to clean it off the silver before dropping into the pickle pot or it will coat the object with a very light copper coating which will polish off easy enough,but prior cleaning will prevent it.I also keep a very fine cheese grater on my bench for grating the red rouge and making myself a little batch to mix with alcohol, makes a creamy paste.Also, in regard to paste solder, I use a small hair dryer on low to soften the paste solder.As soon as my supply is gone, I won't have the problem, I will order from Beth Katz,hers has a proven track record for quality and long shelf life.Usual disclaimers, :-) best wishes, John Barton ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2007, The Ganoksin
Project