Fran

    Welcome. 

>     What are good heat-resistant surfaces to use under a charcoal block
>     or annealing pan? Rio sells 12-inch by 12-inch Silquar(TM)
>     High-Heat Blocks for $21.50 U.S., rated to a maximum temperature
>     of 2000 degrees F (1093 C) -- is that a good choice? What type of
>     fire extinguisher is best to keep nearby when using butane? 

    The block from Rio you sited is similar to what I use, when
    concentrating on soldering it is good to have the extra protection a
    larger surface to work on. 

    On the fire extinguisher, I would use a C or one of the other clean
    ones as you will be in the room with it. I have put out fires with
    the ABC types and what a mess. On a car or trailer not that big a
    deal and on liquids it is my preference, but should you ever have to
    use it in the house, that white powder goes every where. 

Terry
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project