    Okay, Okay.... I know we have all had fire-scale problems in the past
    but I seem to be running into them more lately because I have been
    using multiple layers of very heavy gauge metal for some new pieces I
    have been working on. Usually if I get a little fire-scale I use
    bobbing compound to get rid of it and this has worked well for small
    amounts. However, I am running into much larger amounts in these new
    pieces and it is taking forever to remove it with bobbing compound.
    In addition, the bobbing compound is removing the chasing that I put
    onto the pieces. I have searched high and low for a good
    anti-firescale solution and I keep finding articles that mention
    Prips flux. I pulled the recipe and tried making some but I don't
    think it has turned out right. I desolved the boric acid, borax, and
    tri-sodium phosphate in boiling water. It looked good until the next
    day when I went to use it the solution had crystallized. Has anyone
    had experience making and using this solution? Does it really work?
    Any tips or tricks on dealing with fire-scale would be much
    appreciated. 

Thank you,
Delias
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project