My Orchid friend...Sam Trump

    "Magnetic Tumbling" is a well known process where fine steel "shots"
    or beads of steel are put into a hard plastic container. All of the
    new castings are placed into this receptacle, and again, placed on a
    flat plate. With the aid of the steel shots are added cleaning
    solutions that 'aid' the tumbling and cleaning process. UNDER and in
    this 'Flat plate' is a strong magnet that revolves around in a
    circle. The strong magnetic 'attracts' the steel shots, and tumbles
    the rings and other items with the steel shots over and over again.
    This tumbling action IN THE PLASTIC container will give a satisfactory
    shine to he new castings. Many new casting companies supply this
    service as an added bonus to its customers. Also, many jewelry
    companies have elected to use this method prior to the delicate
    pre-polishing and finishing. 

    The rotary tumbling action in a overnight process took literally
    overnight. But this 'almost' new process takes only 1/2 hour
    maximum!!!! Rotary tumbling creates a waste of time, waste of
    electricity, but it still does not compare to the 'magnetic tumbling'
    process of today. This new method will allow steady watching to its
    completion, by the administrator, all during this tumbling process.
    Have I cleared the air on this topic? Gerry Lewy!..:>)
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project