    I was involved for a few years in developing a large vacum casting
    system for a sculptural foundry and I developed a system for getting
    flasks in and out of a top loading kiln. To give you some idea we
    were using flasks up to 20" high and 10" across, some used 3-4 bags
    of plaster each.

    To lift in and out I drilled a pair of 1/4" holes 1" in from each
    end across the widest section, ie a diameter. Then cut a piece of
    1/4" stainless steel studding 2" longer than the diameter and bolt in
    place inside and out, this is the bottom of the flask. The other end
    use 1 1/4" ss bolts with the heads on the inside. To lift you make a
    strong wire loop like a bucket handle only with the little loops at
    the end twisted to go sideways  I still use a bucket handle for one
    size of flask!).

    You can drop the flask over your wax model quite easily, and the
    studding supports the plaster at the open end. There is obviously a
    lot more to it than this, the foundry went on to LARGE perforated
    flasks but I still use my system to great effect.

regards,
Tim Blades.
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project