>     Are there any tips (besides altering my design) for getting into
>     really tight places between design elements? I have used all
>     manner of points, tips and knife edges, mostly in hard felt, and
>     generally I am not happy with the result. 

    Hi, Lapidary girl! You can thrum. Take some string, and rub it with
    abrasive (I use a string which is doubled and tied to my bench, one
    length is coated with tripoly and the other with green rouge.) Thread
    it into whatever nooks, holes (like the inside of a bail) or whatever
    you need to polish and saw it back and forth. 

    Second, more elegant solution; consider using different textures and
    finishes on your pieces with the convoluted nooks and crannies, so
    that you do not have to bring them to a high polish. Myself, I rather
    fancy the whiteness of pickled sterling on some of my pieces, and
    will just give it a matte finish by rubbing with baking soda rather
    than polishing off all of that nice whiteness.

Lee
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project