    Wow, everyone, thanks so much for the responses! I haven't checked
    my Ganoksin in a while (but now that I'm sitting in a hotel room at
    JCK I have ample time whilst resting my weary feet), and didn't see
    an immediate response, but did manage to arrive at some of the ideas
    you all have presented. 

    The best resource has been a book titled Prop Builder's Molding &
    Casting by Thurston James, which I purchased at Tap Plastics
    (www.tapplastics.com), which also sells molding supplies, and, as
    the name suggests, all varieties of plastic. I've found this store to
    be a great resource for many things, and definitely recommend the
    book above. It's given me lots of ideas not only for jewelry, but for
    making all kinds of fabulous visual merchandising objects. 

    I haven't actually molded my tealeg yet (can we say procrastinating
    on an annoying project?), but as soon as I do, I'll let you know what
    method worked best (or didn't!) Thanks so much everyone! 

Jalia M. LaNoue
Goldsmith
Spinelle Fine Jewelers
Napa, California
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project