    You don't say really enough about your project - how long is long?,
    how big is big? I'm unclear about the layout of this bezel thing,
    exactly. That doesn't matter a whole lot really, because your problem
    is simple - not enough heat. I made what might be a similar project
    once - a silver box about 4" x 8", and I used two prestolite torches
    with big tips to solder it. You need to get the entire piece of
    silver, bezel, base and all, up to about 90% of soldering temp., and
    that can take a lot of heat. And you don't want to concentrate on the
    solder, because it just won't go until the base is hot. You'll just
    boil the solder and ruin it. I wouldn't use hard solder on a huge box
    top - the heat you will need to flow it well can and likely will fry
    (crystallize) your entire lid. I'd use easy, and then you must
    realize that, like Kevin Costner, if you heat it {enough} it will
    flow. 

http://www.donivanandmaggiora.com
 
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project