    A couple of weeks ago, a customer needed a replacement diamond for a
    small, gent's cluster ring. Upon examination, I noticed that two of
    the stones have a square-shaped "phantoms" directly under their table
    facets. Although not very common, they are a cluster of extremely
    tiny pinpoint crystal inclusions that gather in a cubic shape that
    mimics the diamond's isometric (cubic) crystal system. See two photos
    of them heRe: 

    http://home.bellsouth.net/p/PWP-thedocktor 

    Since these two finished stones are basically the same size, the
    phantoms are also the same size, shape and color, coupled with the
    fact that they made it into the same piece of jewelry, the chances
    are pretty good that they came from the same rough. 

    The customer was very nice about trading me for two stones of better
    clarity and color so that I could add these to my modest gemological
    collection so, they are no longer mounted. 

James S. Duncan, G.G.
James in SoFL
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project