    I am coming into this discussion late, so I do not know who
    originally asked the question. 

    Flush setting fancy shape gemstones is one of the most difficult
    setting jobs and should be reserved for someone with experience in
    all forms of stone setting. 

    For someone that would like to accomplish the look of flush setting
    a fancy shape gemstone without the pitfalls that are common with this
    type of job they might consider doing a reverse setting or back set
    method. A back set gemstone is done by carving out the opening in the
    model to accommodate the stone and placing the gemstone into the ring
    from underneath. The crown edge and girdle sit into a seat and then
    just below the girdle would be tab shaped prongs that are pushed up
    to the gemstone to hold it in place. 

    I would not use this type of setting for a high end custom job but
    it might be appropriate for a job that has a price conscience client. 

Greg DeMark
greg AT demarkjewelry
www.demarkjewelry.com
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project