    Technically you can flush-set pretty much any shape of stone, but
    the more sides the stone has, the more complicated and picky the
    setting is (getting it to sit level, protecting all 8 corners from
    chipping, etc.). It also becomes more difficult and risky with stones
    larger than, say, 4mm diameter or so. The other thing to consider is
    that with a larger stone, the culet will end up hanging out the
    underside of the piece, so you would need to design a ring to have
    the stone sit relatively high off the finger anyway. If you are going
    to set the stones yourself, it will benefit you greatly to do some
    practice pieces with CZs the same shape as your stones to get the
    hang of it. If you're sending the setting out to a full-time setter,
    go and ask their advice. The easier you can make life for your
    stonesetter (even if it's you), the lower the expense and aggravation
    for everybody. 

    You might also think about using a heavy bezel-style setting in a
    cast ring - you can get close to the look of flush-setting with the
    stone at the same height it would be if it really were flush-set, and
    it is *way* easier. 

Best of luck!
Laurel Cavanaugh
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project