>     A place I used to work for used black nail polish behind stones
>     like moonstones and opal to bring out the flash. It lasted better
>     than the standard black max or liver of sulfur 

    I gotta say, I can't accept this statement. Left to itself, silver
    eventually turns black, and never turns back to any other color, so
    how can the black "not last", especially behind a moonstone?
    Personally, I think it is a bad idea to use a product that is not
    meant to be permanent (nail polish) for a permanent application. 

    For behind stones, when you want a bright reflection, polished fine
    silver is good, or a piece of mylar from a candy wrapper-- that stuff
    will never rot! For black, I like chemical blackeners like Black
    Max, or for deepest black, I have cut a piece of black plastic from
    one of those little envelopes stones sometimes come in. 

    I guess I could see using black oil paint, since we know oil paint
    lasts for centuries, but not nail polish. 

Noel
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project