From: John Donivan Date: Thu Apr 13 00:03:24 2006 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Although it is possible to etch through metal, and you may even want to try it, it's very tricky to do. Everything has to be just so, to get the piercing without messing up the surface, or piercing too much in the wrong places. There are other options - I can't refer you, but there are etching services that have spray etchers and such. There's also water blast, laser, and the like. All of which, of course, costs money. But I have done much piercing, and I know how laborious it can be. However, I've also played around with etching, and it's perfectly capable of doing what you want, after a LOT of trial and error and practice. And setting up an etching department - acids, resists, fumes, etc. ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project