Dear Kay,

    The Red German pitch is perfect for raising low to medium height
    relief mainly for jewelry. It is not recommended for raising images
    higher than half an inch. For high relief you will need the soft
    grade Northwest pitch. You can still use the Red German pitch for
    raising relatively high relief, just anneal the metal more often and
    place it back into the depression left on the pitch by the previous
    raising. You may also add small amounts of paraffine (material used
    for making candles) into your Red German pitch to make it softer. 

    Another way of raising high relief is to work over thick rubber pad.
    In both cases frequent annealing is essential to preventing the metal
    from breaking. 

Valentin Yotkov

Valentin Yotkov Studio
Artisan Member of Society of American Silversmiths
68 Jay Street, Studio 501A
Brooklyn, New York, 11201
http://www.valentinyotkov.com
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project