>     The big difference between the cheap and the expensive versions
>     are how thick of a piece you can run through it. The good ones from
>     some posts on the similar subject and web searches say they would
>     do about 6 mm, mine will only do about 2.5 mm and mine as well as
>     the two you >mentioned only do half round wire as they come, some
>     of the others can do full round. >.079 is a little over 2mm 

    And that is my concern. The harbor freight one looks tempting but
    the problem is that it will only handle up to 12 gage. I want to do
    texturing and you have to take into account the thickness of the
    metal you are working with. The thickness of what you are using to
    provide the texture. And a brass sheet to protect the roller on the
    texture pattern side. I am afraid that with only 2 mm you will not be
    able to do texture patterns and keep your rollers safe. 

    Maybe some who have used the 2mm models could comment. 

Mark
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project