========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Keo, While I don't have the long term expertise that many of our fellow Orchidians do, I do have a tiny bit of practical experience. My husband bought me a plat900 for our anniversary 4 years ago and I can tell you I am thrilled with it. The band is carved with intricate leaves and stuff (maker is Simon G). I've worn it non-stop. I often forget to remove it for bathing, doing dishes, or working around the house or whatever. If I look very, very closely some of the really delicate lines are maybe slightly blurred, but otherwise the ring is every bit as gorgeous as the day it was put on my finger. Many blessings with your decision, Dawn B. in Taylor, Texas ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project