From: K L Date: Sun Mar 05 21:41:04 2006 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Hi Matthias, Thanks for the pic (via email). Your ring is very nice, not too domed or too flat -very classical indeed. The many scratches, all in all, actually don't look bad at all and produces some matte finish that isn't obvious when looking at it from a distance. I was initially little surprised by the photo, given the alloy /increased hardness of your ring, how scratches were all over it, but none of that really matters any more. If I want some truly scratch-resistant jewelry, there's only RADO. :) I didn't know re-sizing the ring was part of the cold work and that it would render a greater hardness! Cool! Thanks for sharing. My fingers actually expand considerably during hot summer days compared to during winter but what you've recommended is something I have to keep in mind when ordering the ring. I tend to wear my rings little loose. I have an old gold ring that is little too big (19 mm diameter) which I put on today and I shook my hand crazily just to see how secure it'd stay on the finger. It almost fell off. I can easily imagine a heavier platinum ring falling off if not sized properly! (i might go for 18.5 mm or even 18!) About the price level in Germany you mentioned in your previous post: A funny thing that a local jeweler told me just couple of days ago, is that the price difference between 1000 parts plat. and 950/50 plat/palladium is virtually none since palladium isn't that cheap, while other (Japanese) shops quoted a 20% higher price when choosing 1000 parts plat. instead of 950/50. Best rgds, Keo ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project