From: Howard Woods Date: Sun Mar 05 21:40:48 2006 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== > MMA has the structure H2C=C(CH3)COOCH3, while a typical > cyanoacrylate has a structure H2C=C(CN)COOCH3. They differ by the > substitution of a -CN group for a -CH3. This substitution makes it > easier for the material to polymerize into long carbon chains, > much like a zipper closes. OK, you aroused my curiosity! I found a > link for the precise mechanism of the reaction: > www.campoly.com/notes/001.PDF It appears that the autoionization of water provides a weak base to initiate the reaction. Of course, I had to experiment. I dipped a dull burr in household ammonia and applied it to a bead of super glue. As expected, it really speeds up cure time. I would expect more polymer chains each with shorter length with using a surplus of hydroxide ions since one ion is needed for each chain. The bond may be weaker but it shouldn't make much difference for temporary applications. As always, I make a practice of not inhaling anything that comes from the soldering process. Howard Woods Watching another beautiful sunrise in Eagle Idaho. ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project