Keo,

    I'm not sure whether you're an annoying customer but I think you're
    losing sight of the trees in the forest (or whatever that quote is).
    You're buying rings that have importance for their meaning, not
    their content in this case. You are buying rings that symbolize your
    commitment to your partner. There is nothing that will take the
    romance more out of that experience than over analyzing what you're
    buying. I'm not saying you shouldn't have some idea about what
    you're getting, and certainly all stores should disclose what they
    are selling, but if you were my fiancee I'd be mad as heck at you
    that you were spending all this time on what amounts to minute
    differences in the metal instead of getting me a ring I really
    wanted to wear (and if it's an engagement ring, I'd want it now
    instead of in 6 months when you get done deciding what might possibly
    be a metal just slightly better than some other one). 

Daniel R. Spirer, G.G.
Daniel R. Spirer Jewelers, LLC
1780 Massachusetts Ave.
Cambridge, MA 02140
daniel AT spirerjewelers.com
www.spirerjewelers.com

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project