Hi Lynn,

    Pretty bracelet, but yes, 24g is too thin for durable wear.
    Especially those loosely coiled sections will stretch apart. I only
    use 24g when each bead can be held in place by coiling around the
    wire at each end (the hangman's noose thing you mentioned) and almost
    never for a bracelet, because they get much harder wear than
    necklaces. For coils such as you made, 20g hard would be minimal, 22
    for the sections of beads. 

    Your question: "Another wire wrapper from eBay said I should always
    wrap each link (think hangman's noose style wrap) and hide the tail
    ends of wire, and insure better strength. I did not do that for this
    piece, should I have? Do I need to do so always? Have I committed a
    major mistake?" 

    answer-Yes 

Hope that helps, Good luck,
Bev Ludlow
www.wirewrapjeweler.com

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project