    The reply to this thread that I read suggested the like of 950
    Platinum, and another. It is largely a matter of opinion, and
    personal choice, of course. Casters love 950 because of it's flow
    and such. I've worked Platinum intensively for many years, and to me
    there is only one - 10% IrPlat. All of the rest, and believe me, I've
    used each and every one of them, are inferior alloys. If you are
    going to cast a wax, not size it or alter it, and simply polish it
    and put it out, then 950 is OK - it polishes easily and takes a great
    shine (except it's blue). If you want to do anything else, it's
    garbage. 10%Ir is like working in clay or fine wax - the others more
    resemble brass or something. Gas, porosity, surface problems, on and
    on. Not to rant - I guess there are other points of view - I just
    take the position that putting cobalt in platinum is a waste of good
    platinum.....

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project