Hello,

    the liquid I refered to by "bleach", is called "LEJIA" in Spanish:
    it's a colourless liquid (maybe a slight yellow hue) that is in
    every home (at least here) for washing and for cleaning floor
    tiles, specially in bathrooms. When I looked in the dictionary for a
    translation the first word that came up was "bleach". The second
    word was "LYE". If both words refer exactly to the same chemical,
    well, there might be a few "weakened" pieces around in my city.
    However, the "lejia" totally disolved the broken drill bits, and I
    didn't noticed any discoloration on gold (white or yellow, always
    18k) or porosity over the surface or soldered joints. 

    But Please, Please, if lye is the same as bleach, let me know to
    stop using this way of disolving ferrous bits on gold. 

Fernando F. Escudero, Spain.

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project