Hi Augest,

    It is just the way wax appears when patching areas. It is normal for
    wax repairs, and can a good thing to keep track of how many errors
    you make on pieces. I believe it occurs due to the difference in
    molecular structure and in the way light is reflected. The marks
    become more apparent if the pieces are cast waxes, or prefab sheets
    or ring wax, as they were cast at a different temperature and
    solidify in a different way in comparison to the repair wax you're
    filling divots with (warmed by hand or by heated tools). 

    The marks will show up in the wax, but will not show up in your
    final metal design. It can be a pain at times to be sure of accuracy
    with the shape you desire when you have lighter blotches of wax in
    areas, it just takes time to know when its corrected by feeling the
    surface for a smooth surface. 

    I can't stress enough how important it is-- if you are unsure if
    you've properly filled the divot, it is far better to overfill the
    divot than underfill it. You can always sand down excess metal, but
    it is a nightmare to remove a divot when after it is in metal. 

    A little more detailed than necessary, but hope that helps! 

Jim Sprague Jr.

 
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project