From: Paul Ewing
Date: Mon Feb 06 05:02:36 2006
 
     
========[ Invite a Friend - http://www.ganoksin.com/invite.htm  ]========

    Stepped bezels are used most often in open backed settings. The step
    supports the stone. My problem is that I feel the step area is not
    really wie enough for anything be very small stones, so I just make
    my own steped bezel out of a piece of square wire and regular bezel
    wire. 

    Most people use fine silver (.999) for their bezels because it is
    easier to burnish against the stone. You can use sterling if you
    want, and depending on what size of bezel you want, sterling may be
    all you can find from Rio. Personally I like a thicker fine silver
    bezel than Rio stocks. I used to get a 26 guage from Swest before
    Stuller closed them down which was very nice for my larger pieces. I
    refuse to fight with Stuller's strange and complicated ordering
    process so I am having to adjust to the lighter guages that Rio
    offers. Maybe I will check H&S and see if they have a thicker fine
    silver bezel wire available. 

Cheers,
Paul


 
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project