Bill,

    If you are going to vacuum cast I favor the Kerr electro melt
    furnace over a torch for the following reasons: 1. The electro melt is
    easier to use. Put the metal into the crucible and let the furnace
    work. If you buy the electronically controlled unit you can do other
    things while the metal heats up. The furnace will heat the metal to
    your selected temperature then hold it there. If you buy the manually
    controlled unit you will have to monitor the melt closer. You have to
    set the control so that the unit does not burn itself up. 

    2. Temperature control of the electro melt is better. The temperature
    of the metal at the time of the pour will be more consistent with the
    electro melt than with a torch. The thermocouple will monitor the
    temperature in an electro melt. Your eye ball monitors the
    temperature when melting with a torch. 

    3. The electro melt is safer to use. Pouring the metal from an
    electro melt is as easy as pouring coffee from a cup. You do not have
    to handle a very hot crucible with tongs as you pour. 

    4. Ease of melting large amounts of metal. The smaller electro melt
    will felt around 20 ounces of silver at a time. Melting that amount to
    metal with a torch is much more difficult. 

    5. Metal is melted in a reducing atmosphere in the electro melt. 

    There is a less expensive melt furnace on the market that requires
    removing the crucible from the furnace with a pair of tongs when
    pouring the metal. I recommend you stay away from this one. I
    recently wrote a post comparing the two melt furnaces. You might want
    to check that post out. 

    All that being said the electro melt is expensive and you will still
    need a torch for any soldering jobs. 

    If you are going to centrifugally cast the torch would be a better
    idea. 

Lee Epperson


 
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project