Mark-

    The type of plastic/rubber/stuff you use is dependent upon many
    factors, mostly how much detail you need and if you "contain" the
    flow of the plastic. A great source of information is Bonneydoon
    engendering (http://www.bonnydoonengineering.com), I know it has been
    sold, I think Phil Poirier is now in charge. They sell urethane,
    presses and accessories and have a discussion list which would be a
    great source of knowledge. Cynthia Eid, Dar Shelton and Jim Binnion
    who post on this list are also VERY knowledgeable on this subject. 

    It would also be possible to make the other half of the die with
    metal reinforced epoxy if you are pressing soft metal like annealed
    sterling silver. 

    If you are in Denver, I have a Bonneydoon 20 ton press with a variety
    of urethanes if you want to try something out. (marlin at cohrs dot
    org) 


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project