From: FRANKGO Date: Sun Jan 29 12:41:29 2006 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== I have to agree here on both points. The 1350 is too hot 1250 is my max temp and I would try casting around 600-650 for a heavy belt buckle. You might also consider placing your sprue so that the metal is directed toward the back of the buckle if you have not already done this. This allows the most forceful part of the metal delivery directed at the back instead of the smooth front. Less turbulance means a cleaner casting. You might also add a vent sprue to the opposite end of the casting to allow for gas expulsion. I always(even when centrifical casting) use vaculiners to assist in gas expulsion.. my thoughts. Hope they help. Frank ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project