>     James, one of the reasons for buying a puk was for repairing
>     billets and sheet during rolling rather than use solder which could
>     lead to problems when soldering the Mokume gane into pieces of
>     jewellery. Am I right in my thinking? 

    In 20 odd years I have yet to figure out how to repair a
    delaminating billet. You either got it right or you will fight it
    through out the whole damn process and still end up with a sub
    standard product. My normal solution for a delaminating billet is to
    send it out for refining or if it is base metal it goes into the
    scrap bucket. 

>     Mokume Gane apart, I think the Puk opens a new field for jewellery
>     design being able to use stones,pearls,Titanium etc in other ways
>     than up till now. So far I have only seen a Puk demonstated at a
>     trade fair by a salesman (not a jeweller) my tool dealer as yet has
>     not sold one so I have been unable to get a jewellers opinion
>     (until now). 

    I believe there is lots to be explored with using the PUK I am just
    starting to see some things that I can do with it. 

James Binnion
jbin AT mokume-gane.com
James Binnion Metal Arts
http://www.mokume-gane.com
360-756-6550



 
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project