========[ Invite a Friend - http://www.ganoksin.com/invite.htm  ]========

>     Will as reticulate? (After usual depletion guilding.) Also can one
>     enamel over it, without depletion guilding.....or with depletion
>     guilding? I'm not going to ask if it will stand soldering with IT
>     or with eutectic solder without melting; that would be too good to
>     be true!!!! 

    Tom, I wrote a technical article about Argentium Sterling that was
    published by SNAG News. (Every SNAG member receives the newsletter.
    SNAG is at www.snagmetalsmith.org 

    The article is on my website, which is at http://www.cynthiaeid.com/ 

    I recently updated the article, and Rio is publishing it in booklet
    form. There will be copies available at Rio Grande's Catalog in
    Motion in Tucson----I'll be there at the Argentium booth in the
    ballroom, demoing, and answering questions about Argentium Sterling.
    I would love to meet other Orchidians! 

    There is also a lot of information in Trevor's blog, which is at
    http://www.touchmetal.com/blog/argentium-blog.html 

    Argentium Sterling does not reticulate anywhere nearly as well as
    800/200 alloy, which is sold as reticulation silver. 

    Currently, Argentium Sterling is difficult to enamel on due to its
    lower melting point. Peter Johns and Stern-Leach are working on a
    suitable formulation of Argentium Sterling with a higher melting
    temperature that will be more suitable to enameling. 

Cynthia Eid
http://www.cynthiaeid.com/


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project