From: Grace & Tom Stokes
Date: Mon Jan 23 19:06:09 2006
 
     
========[ Invite a Friend - http://www.ganoksin.com/invite.htm  ]========

    OK guys, I thought it would be nice have tarnish free earwires and
    head pins so I took some 20 gauge AS wire, balled up the ends,
    pickled it then put it into a pyrex dish, no cover, into my
    pre-heated 500 degree oven for approximately 2-1/2 hours. It came
    out nearly as soft as when I put it in - no perceptible change in
    temper - no spring at all. I think I tried this once before too and
    it failed but since everyone is saying you can do this in your home
    oven I thought I would try it again. Other than nicely heating up my
    kitchen (thank God it's not summer) I got nowhere..... can anyone
    tell me what I am doing wrong?? 

Grace S.

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project