Terry,

>     have you tried welding with AS yet, no bubbles like SS, the pieces
>     just seem to reach out and touch and merge and it's so slow at
>     transition. I have not seen any ill effects from this yet, have
>     you? I find this easier to control than soldering especially on
>     jump rings and putting a filet on bezel bases. I have started
>     rolling my own bezel material of AS, if the stone will take the
>     heat, I put the stone in with it, if not I just wrestle with the
>     burnisher unit it is set. A post a couple of days ago made me think
>     to try that, and it worked.

    Up till now I had been avoiding using 100% AS on pieces because I
    didn't think I could harden them sufficiently in my household oven -
    now I will most likely switch completely over to AS, except for
    Bezels and gold accents of course. 

    Your question about 'welding' AS - I assume you mean fusing?? No, I
    have not tried any fusing with argentium, but I will, especially
    with jump rings - I just hate trying to get that tiny little piece
    of solder to hit the join - it always creates a bump. I'm sure
    someone else has already done this and could comment from
    experience. Quite honestly I have not done much sweat soldering with
    AS either, but assume there would be not problems provided the fit
    was good and you didn't get too hot. 

Grace S.

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project