>     problems. So far, from responses it doesn't sound like anyone else
>     ever has this problem 

    Yep, I've never had this problem. 

>     - there must be some variable, something I am doing differently
>     which is causing it. Do you clean your pieces before applying
>     patina?? Maybe I am leaving a crucial step out ?? Also, do you use
>     any additives, such as amonia? 

    Yes, pieces should be clean and polished. Patina is the very, very
    last step. No, I don't use ammonia unless I'm doing the iridescent
    plan ala Katherine P. 

    I like the suggestion of a previous poster, use ice water to stop
    the action and dip both earrings at the same time (put them on a wire
    maybe). As I said, I don't normally dip, but in this case it seems
    like a good idea to try to solve your problem. 

    If all else fails, you could use a different product, such as Black
    Max. 

    Good luck! 

Elaine
Elaine Luther
Metalsmith, Certified PMC Instructor
http://www.CreativeTextureTools.com (TM)
Hard to Find Tools for Metal Clay

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project