    Carrie - a flow thru system is usually done with a limited water
    source - mine is 5 gallons. The solution goes thru the tumbler and
    out the bottom to the original 5 gallon bucket. An aquarium pump is
    located above the bottom of the bucket to avoid recycling the junk
    that was washed out of the tumbler. My pump support is made of some
    perforated plastic held together with electrical ties. Most of the
    medium to medium fine media will give you a nice matt finish. You
    can run a closed system with water in the media, but you run the risk
    of having the liquid get gunked up and fowling up your jewelry. The
    alternative is to stop the tumbler every couple of hours, drain the
    liquid, refill it, and run some more. IMHO it's a whole lot easier
    to recycle the rinse water with a flow-thru system. 

    And by the way - you never put the rinse water down the sink - it
    will clog your plumbing in a very short time.

    And to answer your question about the tumbler on the Dillon site,
    that is for dry finishing cartridges. Without major modification, it
    will not run a flow thru system. Running abrasive media dry is not a
    good idea - where does the stuff you abrade going? 

Judy Hoch

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project